typical stress-strain curve

Typical Stress-Strain Curve

For many years, steel producers and stamping plants have gathered the mechanical properties of sheet metal. Individuals recorded properties such as yield strength, n-value and R-value to name a few. As new materials are introduced into the stamping plants, new mechanical properties tests are being discussed. The current use of aluminum and Dual Phase steels has highlighted issues that were insufficiently described by the typical or standard values provided by the tensile test: edge cracking and variation in springback from run to run are two examples. Resulting outcomes can encompass excessive scrap, excessive re-working of parts to remove edge cracks, and even result in excessive downtime as die makers try to correct the issue. The introduction of increasingly complex and sophisticated materials will exacerbate the inefficiencies of the current stamping process. The learning curve can be frustrating.

Proper training for your workforce regarding material mechanical properties and the know-how to develop robust stamping recipes for Advanced High-Strength Steel (AHSS) will benefit the plant. The typical tensile test provides the yield strength, ultimate tensile strength, n-value, uniform and total elongation. And typically, a strain analysis is performed, producing a forming limit diagram to measure a material’s formability. But these tests are reflective of global forming behaviors and don’t adequately describe an advanced material’s performance in localized formability. We need to ask if typical mechanical properties provide adequate information to truly assess the impact to the stamping operation – and if not, what new tests will provide insight on how these materials react to certain forming loads.

Instantaneous n-value

Instantaneous n-value

A new output is instantaneous n-value. Instantaneous n-value identifies the strain gradient – how the material will work-harden at initial contact with the die geometry. If only the standard n-value (work hardening exponent) is observed, measured between 10% and 20% strain, the increase in work hardening that occurs during deformation will be missed. Hole expansion and three-point bend tests are now commonly performed. The hole expansion test identifies the materials ability to stretch at the sheared edge. The three-point bend test identifies the stretchablity of a material via the minimum bend radius that can be achieved for that specific material.

Focusing on AHSS, these materials are characterized by multiple phase structures designed to improve formability. These designer steels are being created to improve crash worthiness through higher strength and lighter gauge thicknesses. To build upon the current understanding of material mechanical properties and resulting forming behaviors, training on AHSS products, testing and stamping process countermeasures is encouraged.

 

 

Related Posts
Filter by
Post Page
Production Managers Tool & Die Professionals homepage-featured-top main-blog Steel Grades AHSS Blog 1stGen AHSS 3rdGen AHSS 2ndGen AHSS Resistance Welding Steel to Aluminium Laser Welding Arc Welding RSW Modelling and Performance Forming Joining
Sort by

Stronger AHSS Knowledge Required for Metal Stampers

This month’s blog was contributed by

18

What are 3rd Gen AHSS?

One of the tasks we took great care in completing during the update of the AHSS Application Guidelines was to

18

Servo Press Force and Energy Considerations When Working With AHSS

Advanced High-Strength Steel (AHSS) products have significantly different forming characteristics and these

18

Process, Microstructure and Fracture Mode of Thick Stack-Ups of Aluminum Alloy to AHSS Dissimilar Spot Joints

This article summarizes a paper entitled, “Process, Microstructure and Fracture Mode of Thick Stack-Ups of

18

Improvement of Delayed Cracking in Laser Weld of AHSS and 980 3rd Gen AHSS

This article is a summary of the paper entitled, “IMPROVEMENT OF DELAYED CRACKING IN LASER WELD OF AHSS AND

18

GMAW of Dissimilar AHSS Sheets

This is a summary of a paper of the same title, authored by K. Májlinger, E. Kalácska, and P. Russo Spena, used by p

18

Modelling RSW of AHSS

Modelling resistance spot welding can help to understand the process and drive innovation by asking the right

18

Forming and Formability of AHSS

Introduction Approaches for forming higher strength steels evolved with the commercialization of increased

18

Role of Coatings in the Formation of Defects in AHSS Welds

A common issue when welding Advanced High-Strength Steels (AHSS) is with protective coatings causing weld defects. A

18